Impact Test: Where the Hammer Falls Decides More Than How Hard

Impact testing looks like the simplest mechanical test: drop a known energy on the sample and see whether it breaks. The energy is specified, the hammer is specified, and the result is pass or fail. What is not fully specified — and what decides the result — is exactly where the hammer lands.

What the rating states

An IK rating states the impact energy an enclosure withstands without damage that would impair safety. The energies run from below 1 J to about 20 J, and each level corresponds to a hammer mass and drop height.

The rating is a property of the enclosure as tested, at the points tested. It is not a property of the material, and it is not uniform over the surface.

LocationStructure behindRelative strength
over a ribstiffenedstrong
flat panel centreunsupported spanweak
next to an openingstress concentrationweakest

Why the weakest point is the honest test

The standard requires impact at the most vulnerable points, not at convenient ones. A panel centre is convenient and usually the weakest — which is why it is often avoided in internal pre-tests where the goal is to pass.

The vulnerable points are: the centre of a large unsupported area, the edge of any opening, the area around a fastener, and any point where the wall thickness changes. Those are the points a dropped object or a knock in service will find.

How the support changes the answer

A sample lying on a bench distributes impact energy into the bench. A sample mounted as it would be in service absorbs it into its own structure. The same energy produces different damage.

This is why the standard specifies the mounting. A product tested free-standing and then installed on a rigid wall has been tested under conditions more severe than service in one sense (no backing) and less severe in another (the wall transmits shock). Neither is obviously conservative.

What counts as failure

Failure is not "the enclosure cracked". It is damage that impairs safety: a live part becoming accessible, a barrier ceasing to separate, a gap opening beyond the probe limit, or a part loosening enough to create a hazard.

A crack that does not create access is a cosmetic result. A hairline gap that admits a test finger is a failure with no visible damage at all — which is why the post-impact inspection uses probes, not eyes.

The inspection that follows

After each impact: check with the relevant probe at the impact point, check that no live part has become accessible, and check that the enclosure still holds together under light manual force.

Recording only "no visible damage" hides the failures that matter. The record should state which probe was applied and at which point.

Practical notes

Hammer condition matters: a worn striking face delivers a different energy distribution than a new one, and a hammer whose release mechanism has been adjusted delivers less than its nominal energy. Calibrate the hammer on a reference sample, not by trusting the scale.

Temperature affects polymers significantly. A test at 23 °C on a material that will see −10 °C in service is optimistic, and the standard for outdoor products accounts for it.