IK Pendulum or Spring Hammer: Choosing the Right Impact Source

An IK rating is a number of joules. How those joules arrive is not specified by the rating, and the two standard instruments deliver them differently enough that a product can pass with one and fail with the other.

The two instruments

The spring hammer releases a compressed spring against a striker held against the sample. The pendulum swings a mass on an arm. Both are calibrated in joules, and both are accepted by IEC 62262.

PropertySpring hammerPendulum
Energy range0.14 to 2 J0.5 to 50 J
Contact durationShort, millisecondsLonger, mass dependent
DirectionAny, hand-heldConstrained to the arc
RepeatabilityGood with a fixtureGood, geometry fixed
Typical useSmall enclosures, IK01 to IK08Large enclosures, IK08 to IK10

Why the results differ

A spring hammer concentrates its energy in a few milliseconds, which produces a high local stress and tends to crack brittle materials. A pendulum delivers the same energy over a longer contact, which deforms ductile materials and tends to produce dents and permanent set.

A polycarbonate window that survives a 2 J spring hammer can dent under a 2 J pendulum, and the dent may be the failure if the criterion is no permanent deformation.

Choosing, and saying which

Choose the instrument the product standard names. Where the standard allows either, choose the one that matches the service environment: dropped tools favour the spring hammer, a swinging door or a forklift favours the pendulum.

And write the instrument into the report. An IK08 claim without naming the impact source is not reproducible, and two labs will produce two different results on the same sample.

Standards referenced: IEC 62262 for IK ratings, IEC 60068-2-75 for the spring hammer, IEC 60068-2-75 Annex for pendulum guidance.

The striker tip and the damage it makes

Both instruments use a hardened steel striker, but the tip geometry differs: the spring hammer typically uses a 10 mm radius hemispherical tip, the pendulum a larger radius or a flat face depending on the standard.

A smaller radius concentrates stress and produces cracking; a larger radius distributes load and produces denting. The same energy therefore produces different damage, and the acceptance criterion follows the damage type.

Conditioning before the test

Impact results depend on temperature. A polycarbonate enclosure at 20 °C dents; the same enclosure at −10 °C cracks. Unless the product standard says otherwise, condition the sample at 23 ± 2 °C for at least 4 hours before impact.

Record the conditioning. An impact result without a temperature is not reproducible, especially for polymers near their glass transition.

What to do with a marginal result

A single crack at the maximum energy is a design question, not a test question. Increasing wall thickness by 0.5 mm or adding a rib often moves the result by a full IK level, and it is cheaper than changing material.

Mounting is half the result

A sample held rigidly transfers the full energy into the material; one that can move absorbs some of it. The standard requires the sample to be mounted as in normal use, which for a wall-mounted enclosure means on a rigid wall, not on a bench.

A 5 kg sample free to move on a bench can absorb 20 % or more of a 2 J impact, which flatters the result. Bolt it down or back it with a rigid mass.