Home News

Ball Pressure Test: What a 5 mm Ball at 20 N Actually Measures

Ball Pressure Test: What a 5 mm Ball at 20 N Actually Measures

Good quality IEC 60065 Standard for sales
Good quality IEC 60065 Standard for sales
Our goods has safely arrived at our residence. Thank you for your excellent services. I hope we can cooperate again in the future.

—— Wira

I'm Online Chat Now
Ball Pressure Test: What a 5 mm Ball at 20 N Actually Measures

A steel ball, 5 mm in diameter, pressed into a plastic part with a 20 N load for one hour at a set temperature. Afterwards the depth of the dimple is measured. That is the whole test, and it answers a question that no datasheet answers directly: does this material stay stiff enough at working temperature to keep its shape?

The apparatus and the numbers

The test is defined in IEC 60695-10-2. The loaded ball is 5 mm diameter, the force is 20 N, the duration is one hour, and the part is at a temperature specified by the product standard. After the hour the ball is removed and the dimple diameter is measured; a result of 2 mm or less is the usual acceptance.

ParameterValueWhy it matters
ball diameter5 mmsets the contact stress
force20 Nabout the load of a small component
duration1 hallows creep, not just elastic give
dimple2 mm maxthe acceptance criterion

What the temperatures mean

The temperature is not a property of the material; it is a property of the application. Product standards set it by function. Parts that support live parts are tested at a higher temperature than decorative or external parts, because a support that yields lets a live part move.

Typical figures quoted in appliance standards are 75 °C for parts not supporting live parts and 125 °C for those that do, but the exact value is stated in the product standard, and copying the number from another product family is how a qualification ends up testing the wrong thing.

Why one hour, and why creep matters

Thermoplastics do not fail by instant yielding at these loads. They creep: the dimple grows slowly while the load is applied, and most of the growth happens in the first minutes but continues.

A ten-minute test would pass materials that fail at an hour. That is why the duration is fixed, and why a shortened test cannot be presented as equivalent. It is also why the test is run at equilibrium temperature — a part that is still warming is not at the temperature the standard specifies.

Where the ball goes

The test is applied to the surface that will see the load in service, and on a moulded part that is rarely the flat outer face. The relevant locations are:

Where a component rests. A terminal block bolted to a boss presses on that boss for life.

Thin sections near a heat source. A wall 1.5 mm thick next to a transformer is at a higher temperature than the ambient the part was tested at.

Supporting ribs. A rib carries load on a narrow edge, and the contact stress there is higher than on a flat face for the same force.

Testing the most convenient flat area and calling it a pass is the most common error in this test, and it is invisible in the report.

Reading the result

The dimple diameter is measured, not the depth, in most standards — and the two are related but not equivalent. A dimple of exactly 2 mm with a clean edge is a pass; a smaller dimple with radial cracking around it may be a failure, because cracking indicates the material has lost cohesion rather than simply deformed.

Look at the rim. A dimple with a raised lip has displaced material plastically; a dimple with a crack at the rim has failed in a way the diameter does not capture.

What it does not tell you

Three things this test is often assumed to prove and does not:

It is not a heat resistance test. A material can pass at 125 °C and distort at 100 °C under a different load geometry, because the test's stress state is a point load, not a distributed one.

It is not a flammability test. Nothing about ignition or burning is measured.

It is not a long-term property. One hour at temperature says nothing about 20,000 hours. For that, the material's long-term service data is the relevant source.

Sample preparation

The specimen must be at the test temperature throughout, which means it goes into the oven with the apparatus and stays there for the full hour. A cold specimen placed under a preheated ball gives a result that depends on how long it took to warm up.

The surface must be as produced. A machined flat removes the skin, which on an injection moulding is the most crystalline and stiffest layer — and makes the material look better than the part actually is.